A series of experimental precipitated calcium carbonates (PCCs) coated with commercial stearic acid (stearin), with the coating amount of stearin added to the PCC particles ranging from 3 to 13.5 wt %, were prepared in aqueous medium and characterized by Fourier transform infrared spectroscopy (FTIR), thermogravimetric analysis (TGA), and differential scanning calorimetry (DSC). FTIR and TGA results indicated that only calcium stearate is present without any free stearic acid left on the surface of the produced PCCs. It was also found that the calcium stearate formed on the coated surface is partially chemisorbed and partially physisorbed. Interestingly, the surface coverage oldie chemisorbed stearate, determined by the DSC technique in about 3.25 set %, was much lower than the theoretical run monolayer coverage (4.17 wt %) for the same set of particles. This result was confirmed by determining the amount necessary to cover the filler with a full monolayer of surfactant by means of a dissolution method where the amount of dissolved surface agent, after the coating reaction, was measured by gas chromatography (GC). In other words, a complete chemisorbed monolayer on the surface cannot be reached, even in the presence of an amount of stearate ions far in excess compared to those required by the stoichiometry. This can be explained by considering that the coating in aqueous medium is quite different from solvent or dry coating, since the process is controlled by micelle adsorption, followed by the collapse of micelles into double or multiple layers during the drying stage.

On the Coating of Precipitated Calcium Carbonate with Stearic Acid in Aqueous Medium

LAZZERI, ANDREA
2010-01-01

Abstract

A series of experimental precipitated calcium carbonates (PCCs) coated with commercial stearic acid (stearin), with the coating amount of stearin added to the PCC particles ranging from 3 to 13.5 wt %, were prepared in aqueous medium and characterized by Fourier transform infrared spectroscopy (FTIR), thermogravimetric analysis (TGA), and differential scanning calorimetry (DSC). FTIR and TGA results indicated that only calcium stearate is present without any free stearic acid left on the surface of the produced PCCs. It was also found that the calcium stearate formed on the coated surface is partially chemisorbed and partially physisorbed. Interestingly, the surface coverage oldie chemisorbed stearate, determined by the DSC technique in about 3.25 set %, was much lower than the theoretical run monolayer coverage (4.17 wt %) for the same set of particles. This result was confirmed by determining the amount necessary to cover the filler with a full monolayer of surfactant by means of a dissolution method where the amount of dissolved surface agent, after the coating reaction, was measured by gas chromatography (GC). In other words, a complete chemisorbed monolayer on the surface cannot be reached, even in the presence of an amount of stearate ions far in excess compared to those required by the stoichiometry. This can be explained by considering that the coating in aqueous medium is quite different from solvent or dry coating, since the process is controlled by micelle adsorption, followed by the collapse of micelles into double or multiple layers during the drying stage.
2010
X., Shi; R., Rosa; Lazzeri, Andrea
File in questo prodotto:
File Dimensione Formato  
Langmuir2010.pdf

solo utenti autorizzati

Descrizione: Articolo principale
Tipologia: Versione finale editoriale
Licenza: NON PUBBLICO - Accesso privato/ristretto
Dimensione 1.37 MB
Formato Adobe PDF
1.37 MB Adobe PDF   Visualizza/Apri   Richiedi una copia

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11568/139551
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 95
  • ???jsp.display-item.citation.isi??? 89
social impact