A grating resolution of up to 200 nm is achieved using room-temperature nanoimprint lithography on several different light-emitting low-molar-mass organic semiconductors, without any degradation of the active materials after patterning (see Figure). This could be the only process that permits the transfer of a height profile to films of this very important class of low-molar-mass conjugated molecules with poor thermoplastic behavior.

Room-temperature nanoimprint lithography of non-thermoplastic organic films

PISIGNANO, DARIO
2004-01-01

Abstract

A grating resolution of up to 200 nm is achieved using room-temperature nanoimprint lithography on several different light-emitting low-molar-mass organic semiconductors, without any degradation of the active materials after patterning (see Figure). This could be the only process that permits the transfer of a height profile to films of this very important class of low-molar-mass conjugated molecules with poor thermoplastic behavior.
2004
Pisignano, Dario
File in questo prodotto:
Non ci sono file associati a questo prodotto.

I documenti in IRIS sono protetti da copyright e tutti i diritti sono riservati, salvo diversa indicazione.

Utilizza questo identificativo per citare o creare un link a questo documento: https://hdl.handle.net/11568/886204
Citazioni
  • ???jsp.display-item.citation.pmc??? ND
  • Scopus 71
  • ???jsp.display-item.citation.isi??? 66
social impact